3M 4491
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Low-Viscosity Spray Application
- Optional Heat-Cure Processing
- Water, Fuel, and Oil Resistance
Product Description
3M Nitrile Industrial Adhesive 4491 is a solvent-based nitrile adhesive for flexible bonding of vinyl extrusions and sheeting, fabrics, leather, foam, and many plastics. Its low-viscosity formulation is intended for spray application and dries at room temperature; optional heat curing can increase physical properties. Finished bonds resist weathering, water, oils, fuels, many solvents, and plasticizer migration. Spray coating and flexible bond formation support decorative vinyl attachment to cabinets, wall linings, and flooring, as well as rubber and vinyl floor assemblies.
Key features
- Spray-applied nitrile adhesive: The low-viscosity liquid can be coated onto vinyls, plastics, fabrics, leather, and foam.
- Optional heat curing: Room-temperature drying forms the bond; subsequent heat curing can increase physical properties.
- Fluid and weather resistance: Finished bonds resist water, oils, fuels, many solvents, plasticizer migration, and weathering.
Applications
Cabinet decorative vinyl bonding; wall lining and flooring; rubber and vinyl floor bonding.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
Values are typical and not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive chemistry | Nitrile | - | Solvent-based adhesive |
| Viscosity grade | Low viscosity | - | Sprayable formulation |
| Primary application method | Spray | - | Apply to supported substrates |
| Processing options | Room-temperature drying or heat cure | - | Heat cure can increase physical properties |
After-processing / final-state properties
Values are typical and not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Bond character | Flexible | - | Finished adhesive bond |
| Environmental resistance | Weathering and water | - | Bonded adhesive |
| Fluid resistance | Fuels, oil, and many solvents | - | Bonded adhesive |
| Plasticizer migration | Resistant | - | Finished adhesive bond |